MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mo-Sci Corporation GL 1705 Viscous Glass Seal
Categories: Ceramic; Glass

Material Notes: Viscous glass seals bond to metals and ceramics, but resist crystallization and operate in a viscous state at SOFC operating temperatures. Viscous seals reduce the risk of catastrophic seal failure through viscous healing of cracks if they form during thermal cycling. Applications: To seal ceramics and metals.

Information provided by Mo-Sci Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.20 g/cc0.116 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 µm/m-°C
@Temperature 50.0 - 500 °C
4.44 µin/in-°F
@Temperature 122 - 932 °F
Transformation Temperature, Tg 563 °C1050 °F+/- 10°C
Softening Point 598 °C1110 °FDilatometric +/- 10°C
 
Processing PropertiesMetricEnglishComments
Processing Temperature 800 - 850 °C
@Time 7200 - 14400 sec
1470 - 1560 °F
@Time 2.00 - 4.00 hour
Firing Temp. Heating/cooling rate: 3 to 10°C/min.
 
Component Elements PropertiesMetricEnglishComments
Al2O3 9.91 - 12.11 %9.91 - 12.11 %
B2O3 34.37 - 45.62 %34.37 - 45.62 %
BaO 29.91 - 36.55 %29.91 - 36.55 %
CaO 2.42 - 3.64 %2.42 - 3.64 %
 
Descriptive Properties
CoO (%)0.33 to 0.49
NiO (%)0.66 to 0.98
ZnO (%)3.52 to 5.28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMOSCI9016 / 200231

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.