MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Pressure Seal 3425 Nitrile - Butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 3425 is a 40 durometer white colored Buna N elastomer, it is formulated with FDA sanctioned materials. It will remain non brittle at low temperatures.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BG 410 B14 B34 EA14 EF11 EF21 EO34 F17; 5 BG 410 A14 B14 B34

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45
 40
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 40
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3
 43
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
 44
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
 45
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 45
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1
 56
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged
 56
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
Tensile Strength 1275 psi
 392.7 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 663 psi
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged
 663 psi
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 1081.2 psi
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
 1199.8 psi
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3
 1434.4 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 2176.43 psi
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1
Elongation, Ultimate 641 %
 161.5 %
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged
 161.5 %
@Treatment Temp. 125 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 373.1 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 578.823 %
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aged
 601.3 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3
 653.82 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 683.3 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1
100% Modulus 180 psi
Tear Strength 112 pliDie B; Method D 624
 130 pliDie C; Method D 624
Compression Set 12.6 %
@Treatment Temp. 100 °C,
Time 79200 sec
Solid
 17.9 %
@Treatment Temp. 100 °C,
Time 252000 sec
Solid
 18.2 %
@Treatment Temp. 125 °C,
Time 79200 sec
Solid
 21.3 %
@Treatment Temp. 100 °C,
Time 79200 sec
Plied
 28 %
@Treatment Temp. 100 °C,
Time 252000 sec
Plied
 31.3 %
@Treatment Temp. 125 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -43.0 °F
Shrinkage -9.00 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, ASTM Oil #1
 0.70 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 6.4 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 6.6 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, ASTM Oil #3
 27.7 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel B
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL003 / 318213

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.