System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Huafon JF-P-4170/JF-I-4118 Polyester
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyester TPE
Material Notes:
Characteristics: Low hardness and high density
Applications: For casual shoes and direct injection shoes
Information provided by Zhejiang Haufon New Materials Corp., Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.260
-
0.320
g/cc
0.00939
-
0.0116
lb/in³
Free rise foam density, insole
0.400
-
0.500
g/cc
0.0145
-
0.0181
lb/in³
Free rise foam density, outsole
0.550
-
0.600
g/cc
0.0199
-
0.0217
lb/in³
Molded, insole
0.700
-
0.750
g/cc
0.0253
-
0.0271
lb/in³
Molded, outsole
1.17
-
1.19
g/cc
@Temperature 40.0 °C
0.0423
-
0.0430
lb/in³
@Temperature 104 °F
JF-P-4170
1.18
-
1.20
g/cc
@Temperature 40.0 °C
0.0426
-
0.0434
lb/in³
@Temperature 104 °F
JF-P-4118
Viscosity
200
-
500
cP
@Temperature 40.0 °C
200
-
500
cP
@Temperature 104 °F
JF-P-4118
800
-
1200
cP
@Temperature 40.0 °C
800
-
1200
cP
@Temperature 104 °F
JF-P-4170
Mechanical Properties
Metric
English
Comments
Tensile Strength
>=
5.00
MPa
>=
725
psi
midsole
>=
8.00
MPa
>=
1160
psi
outsole
Elongation at Break
>= 450 %
>= 450 %
midsole
>= 500 %
>= 500 %
outsole
Tear Strength
>=
20.0
kN/m
>=
114
pli
midsole
>=
30.0
kN/m
>=
171
pli
outsole
Abrasion
>= 30
>= 30
[%] NBS abrasion resistance, outsole
Processing Properties
Metric
English
Comments
Mold Temperature
45.0
-
55.0
°C
113
-
131
°F
midsole
50.0
-
55.0
°C
122
-
131
°F
outsole
Descriptive Properties
Appearance
Liquid or waxy
40°C, JF-P-4170
Transparent and pure liquid
40°C, JF-I-4118
Asker A Hardness
45-50
midsole
63-68
outsole
Asker C Hardness
60-65
midsole
80-85
outsole
Cream time
5-7 sec
Demold time
3-5 min
Material Temperature
35-40°C
outsole
38-42°C
midsole
40-45°C
outsole
P+C/l Mix ratio
100/86-88
outsole
100/90-92
midsole
Rise time
25-35 sec
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PHUAF017 / 294960
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.