MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling SUSTANAT® PC MG Polycarbonate Medical Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.35 %0.35 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575ASTM D785
Hardness, Rockwell R 126126ASTM D785
Hardness, Shore D 8080ASTM D2240
Tensile Strength, Yield 68.9 MPa10000 psiASTM D638
Elongation at Break 75 %75 %ASTM D638
Tensile Modulus 2.21 GPa320 ksiASTM D638
Flexural Strength 89.6 MPa13000 psiASTM D790
Flexural Modulus 2.34 GPa340 ksiASTM D790
Izod Impact, Notched 5.34 J/cm10.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.4 µm/m-°C38.0 µin/in-°FASTM D696
Thermal Conductivity 0.187 W/m-K1.30 BTU-in/hr-ft²-°F
Melting Point 154 °C310 °FASTM D789
Maximum Service Temperature, Air 121 °C250 °F
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF NoNo
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling SUSTAPEEK® MG natural Medical Grade PEEK
Röchling SUSTANAT® PC Polycarbonate
Röchling SUSTANAT® PC GF20 Polycarbonate, 20% Glass Reinforced
INEOS Styrolution Luran® S KR 2864C Colored ASA+PC
Ter Hell Plastic Terez® PC X 9005 GF 5 Polycarbonate, 5% Glass Fiber

PROCH9046 / 232749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.