MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Armacell Okabell® PVDF Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Description: Stainless-Steel Roll Jacketing manufactured for AISI-304, AISI-304L, AISI-316 and AISI-316L prime grade Austenitic stainless steel with regular 2B finish for flatness and reduced glare. Smooth surface, suitable for outside application.

Application: Jacketing for insulated pipes (inclu. Bends, fittings, flanges, etc.) to protect against mechanical stress to hostile environment such as refinery and Petro-Chemical applications.

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Taber Abrasion, mg/1000 Cycles 3030[g], 250 rev, CS 10 wheels; EN 13523-16
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
304 Stainless Steel
316 Stainless Steel, annealed sheet
Omnia Plastica Kynar® PVDF
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
ScanTube PVDF Tubing

PARMD172 / 186783

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.