MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teknor Apex Monprene® MP-1736T XRD Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene MP-1736T XRD is a general purpose thermoplastic elastomer designed for a variety of industrial application, including seals and gaskets. Monprene MP-1736T XRD is a low hardness, low density grade that is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Flexibility; Good Processability; High Flow; Light Stabilized; Low Density; Low Specific Gravity; Lubricated; Low Hardness; Sunlight Resistant; Weather Resistant; Without Fillers

Uses: Consumer Applications; Flexible Grips; Gaskets; General Purpose; Grommets; Handles; Plugs; Rubber Replacement; Soft Touch Applications; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792
Melt Flow 45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
45 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  20
@Time 5.00 sec
20
@Time 0.00139 hour
Injection Molded; ASTM D2240
 23
@Time 1.00 sec
23
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 2.80 MPa406 psi20 in/min, Flow; ASTM D412
 3.86 MPa560 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  0.496 MPa
@Strain 100 %
72.0 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 0.807 MPa
@Strain 100 %
117 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 0.979 MPa
@Strain 300 %
142 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 1.29 MPa
@Strain 300 %
187 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 670 %670 %20 in/min, Across Flow; ASTM D412
 790 %790 %20 in/min, Flow; ASTM D412
Tear Strength 12.1 kN/m69.0 pli20 in/min, Flow; ASTM D624
 17.5 kN/m100 pli20 in/min, Across Flow; ASTM D624
Compression Set 19 %
@Temperature 22.8 °C,
Time 79200 sec
19 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 199 - 249 °C390 - 480 °FMelt, Injection
Rear Barrel Temperature 182 - 232 °C360 - 450 °FInjection
Middle Barrel Temperature 188 - 238 °C370 - 460 °FInjection
Front Barrel Temperature 193 - 243 °C380 - 470 °FInjection
Nozzle Temperature 199 - 249 °C390 - 480 °FInjection
Zone 1 182 - 232 °C360 - 450 °FExtrusion
Zone 2 188 - 238 °C370 - 460 °FExtrusion
Zone 3 193 - 243 °C380 - 470 °FExtrusion
Zone 4 193 - 243 °C380 - 470 °FExtrusion
Zone 5 199 - 249 °C390 - 480 °FExtrusion
Die Temperature 199 - 249 °C390 - 480 °FExtrusion
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0875 / 237366

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.