MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Empilon EMPILON® 365 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: EMPILON® 3 series is the entry-level material of EMPILON®, which can be widely used in general products that do not require tensile strength (such as tool handles, daily commodities, sports goods, stationery toys, etc.); It is a mainly blending material, with hardness range between Shore A28 ~ Shore 85, can be processed by injection molding, extrusion molding and calendaring. The series is non-toxic. It does not contain RCRA 8 heavy metals, halogens, phthalate and is 100% recyclable and eco-friendly. It can pass the European Union Waste Electronics and Electrical Equipment (WEEE), Restriction of Hazardous Substances (RoHS) regulations and meet the environmental requirements of SONY SS-00259 4th Edition. It has great chemical resistant and hydrolysis resistant performance. EMPILON® 3 series products need to be dried with hot air at 70-80? (dehumidification and drying is recommended) for at least 2 hours before processing, and drying is required during injection molding process. When you want to dye this series of products, please choose PE or EVA as the substrate of masterbatch, and never use PVC as the base material. In addition, please use a higher screw speed and higher back pressure to achieve better dispersion of the colorant.

Series Features:

  • Wide Hardness Range
  • Non-toxic Material
  • Excellent Low Temperature Property
  • No DOP
  • Chemical Resistance
  • Hydrolysis Resistance
  • Easy to Processing, apply to general usage product
  • Able to process with normal processing methods
  • Apply to daily commodities, gardening tools which owns anti-slip and great tactile feeling product
Applications:
  • Suitcase wheel: Aesthetic/Wear Resistance
  • Daily Commodities: Escalate Tactile Feeling
  • Garden Tools: Anti-slip/Comfortable tactile feeling
  • Anti-slip Handle: Anti-slip/Comfortable tactile feeling
  • Gasket: Aesthetic/Easy to processing

Information provided by EMILON®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Melt Flow >= 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
@Time 10.0 sec
ASTM D2240
Tensile Strength 20.0 kg(f)/cm²ASTM D412
Elongation at Break 400 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -55.0 °C
Shrinkage, MD 1.3 %
Shrinkage, TD 1.1 %
 
Processing PropertiesOriginal ValueComments
Feed Temperature 165 - 175 °C
Middle Barrel Temperature 175 - 185 °C
Front Barrel Temperature 185 - 195 °C
Nozzle Temperature 180 - 190 °C
Melt Temperature 165 - 195 °C
 <= 220 °Cdo not exceed
Mold Temperature 30.0 - 50.0 °C
Injection Pressure 2.94 - 3.92 MPa
Back Pressure 0.490 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEMPIL003 / 294690

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.