Wanhua Chemical Wanthane® WHT-6275 TPU Hot-Melt Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Wide range of activation temperature, fast crystallization rate, outstanding bonding strength for fabrics, leathers, plastics & rubbers, wood, etc.
Information provided by Wanhua Chemical Group Co., Ltd.
Key Words:
FDA 21 CFR 177.1680, 177.2600; RoHS
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
77
77
Thermal Properties
Metric
English
Comments
Softening Point
90.0
°C
194
°F
Flow beginning temperature
Processing Properties
Metric
English
Comments
Tack-Free Time
20.0
min
0.333
hour
Descriptive Properties
Bonding Temperature, °C
110-130
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Braskem Evateno® HM 150 EVA Hot Melt Copolymer
Kuraray SEPTON® A2 Hot Melt Adhesive
Master Bond MB529 Acrylic Polymer Based, Hot Melt Adhesive System
SunChemical Gwent R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors
Kuraray SEPTON® A1 Hot Melt Adhesive
PWANTH940 / 156363
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.