MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Imerys KT Cast™ Kaolin
Categories: Ceramic; Clay; Kaolin Clay; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: KT Cast is a coarse-grained, white firing kaolin that is used primarily in casting bodies based on its fast casting and exceptional deflocculation characteristics.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.50 µm0.50 µm21% finer than
 1.0 µm1.0 µm41% finer than
 2.0 µm2.0 µm60% finer than
 5.0 µm5.0 µm75% finer than
 10 µm10 µm87% finer than
 20 µm20 µm95% finer than
Particle Mesh Size 325 Mesh325 Mesh5.0% retained
pH 5.55.5
Specific Surface Area 12 m²/g12 m²/g
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00155 GPa0.225 ksidry
 
Component Elements PropertiesMetricEnglishComments
Al2O3 38.8 %38.8 %
CaO 0.10 %0.10 %
Carbon, C 0.030 %0.030 %
Fe2O3 0.40 %0.40 %
K2O 0.10 %0.10 %
Loss on Ignition(%) 13.6 %13.6 %
MgO 0.10 %0.10 %
Na2O 0.10 %0.10 %
SiO2 45.1 %45.1 %
Sulfur, S 0.030 %0.030 %
TiO2 1.6 %1.6 %
 
Descriptive Properties
M.B.I. (meq/100g)2.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip
Sapphire Spelling Note
Kaolinite (Al2O3-2SiO2-2H2O)

CIMERY048 / 88398

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.