System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Romira LURANYL® KR 2401 PPE/PS-I
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Polystyrene + Polyphenylene Ether, Unreinforced
Material Notes:
PPE/PS-I, injection moulding grade, impact-resistant, high stiffness
Information provided by Romira
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.06
g/cc
0.0383
lb/in³
50 % RH; DIN EN ISO 1183
Water Absorption
<= 0.10 %
@Time 86400 sec
<= 0.10 %
@Time 24.0 hour
50 % RH; DIN EN ISO 62
Linear Mold Shrinkage
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
DIN EN ISO 294-4
Melt Flow
110
g/10 min
@Load 21.6 kg,
Temperature 250 °C
110
g/10 min
@Load 47.6 lb,
Temperature 482 °F
DIN EN ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength
52.0
MPa
7540
psi
50 mm/min; DIN EN ISO 527
Elongation at Break
4.0 %
4.0 %
50 mm/min; DIN EN ISO 527
Tensile Modulus
2.50
GPa
363
ksi
1 mm/min; DIN EN ISO 527
Flexural Strength
90.0
MPa
13100
psi
2 mm/min; DIN EN ISO 178
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
80 x 10 x 4 mm; DIN EN ISO 179/1eU
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80 x 10 x 4 mm; DIN EN ISO 179/1eU
Charpy Impact, Notched
1.20
J/cm²
@Temperature -30.0 °C
5.71
ft-lb/in²
@Temperature -22.0 °F
80 x 10 x 4 mm; DIN EN ISO 179/1eA
2.00
J/cm²
@Temperature 23.0 °C
9.52
ft-lb/in²
@Temperature 73.4 °F
80 x 10 x 4 mm; DIN EN ISO 179/1eA
Thermal Properties
Metric
English
Comments
CTE, linear
60.0
-
70.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
33.3
-
38.9
µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity
0.180
W/m-K
1.25
BTU-in/hr-ft²-°F
DIN 52612
Deflection Temperature at 1.8 MPa (264 psi)
106
°C
223
°F
DIN EN ISO 75-1
Vicat Softening Point
117
°C
@Load 5.10 kg
243
°F
@Load 11.2 lb
50 °C/h; DIN EN ISO 306
Flammability, UL94
HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
File No.: 148878
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PROMR064 / 280770
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.