Nucleated and long-term aging (LTHA). Produced without animal derived components or phthalates. Applications: Medical and electrical device components Regulatory: FDA – 21 CFR 177.1520(c) 1.1a; USP <88> Class VI, USP<85>, and ISO 10993-5; UL Certified 94HB, UL 746 RTI rated Information provided by INVISTA. |