MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Seals Eastern 7265 Fluorocarbon-Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.

Features:

  • Viton ETP
  • Broad chemical resistant

Viton® is a registered trademark of DuPont. Information provided by Seals Eastern.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/ccASTM D297, 15
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 84>= 84ASTM D2240
 8888Average; ASTM D2240
Tensile Strength >= 13.1 MPa>= 1900 psiASTM D412 Method A
 16.4 MPa2380 psiAverage; ASTM D412 Method A
Tensile Stress at Strain  4.65 MPa
@Strain 25 %
675 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 6.21 MPa
@Strain 50 %
>= 900 psi
@Strain 50 %
ASTM D412 Method A
 7.412 MPa
@Strain 50 %
1075 psi
@Strain 50 %
Average; ASTM D412 Method A
 >= 8.96 MPa
@Strain 100 %
>= 1300 psi
@Strain 100 %
ASTM D412 Method A
 11.20 MPa
@Strain 100 %
1625 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 100 %>= 100 %ASTM D412 Method A
 200 %200 %Average; ASTM D412 Method A
Modulus of Elasticity 0.02948 GPa4.275 ksiCalculated; ASTM D412 Method A
Poissons Ratio 0.500.50Calculated
Shear Modulus 0.009825 GPa1.425 ksiCalculated; ASTM D412 Method A
Secant Modulus 0.02771 GPa4.019 ksiASTM D412 Method A
Tear Strength Test 146146psi; ASTM D624, Die B
Compression Set 44 %
@Temperature 200 °C,
Time 252000 sec
44 %
@Temperature 392 °F,
Time 70.0 hour
ASTM D395, Test B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C200 °F
Glass Transition Temp, Tg -21.1 °C-6.00 °FASTM D1329
 
Processing PropertiesMetricEnglishComments
Shelf Life 240 Month240 Month
 
Descriptive Properties
Strain Energy/ Unit Volume at 20% Elongation (psi)76ASTM D412 Method A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 7265D Fluorocarbon-Elastomer
Seals Eastern 7182B Fluorocarbon-Elastomer

PSEAL907 / 139300

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.