System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Arkema Orgalloy® RS 6630 BLACK Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 30% Glass Fiber Filled
Material Notes:
Polyamide Alloy, Rigid grade, Nylon 6.6 based
Molding of Engineering Parts
Information provided by Arkema Group
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.27
g/cc
ISO 1183
1.27
g/cc
Cond.; ISO 1183
Water Absorption
1.9 %
Dry; Sim. to ISO 62
Moisture Absorption
0.900 %
Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow
0.0030
cm/cm
Dry; ISO 294-4, 2577
0.0070
cm/cm
Melt Flow
7.0
g/10 min
@Load 2.16 kg,
Temperature 275 °C
cm³/10 min Volumetric Rate; ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore D
79
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength at Break
125
MPa
Cond.; ISO 527-1/-2
130
MPa
Dry; ISO 527-1/-2
Elongation at Break
3.0 %
Dry; ISO 527-1/-2
3.0 %
Cond.; ISO 527-1/-2
Tensile Modulus
8500
MPa
Cond.; ISO 527-1/-2
8900
MPa
Dry; ISO 527-1/-2
Charpy Impact Unnotched
NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched
10.0
kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
11.0
kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
Tensile Creep Modulus, 1 hour
7900
MPa
Cond.; ISO 899-1
Tensile Creep Modulus, 1000 hours
5620
MPa
Cond.; ISO 899-1
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
Surface Resistance
>=
1.00e+15
ohm
Cond.; IEC 60093
Dielectric Constant
3.0
@Frequency 100 Hz
Cond.; IEC 60250
4.0
@Frequency 1e+6 Hz
Cond; IEC 60250
Dielectric Strength
34.0
kV/mm
Dry; IEC 60243-1
34.0
kV/mm
Cond.; IEC 60243-1
Dissipation Factor
0.016
@Frequency 1e+6 Hz
Cond.; 0
0.029
@Frequency 100 Hz
Cond.; IEC 60250
Comparative Tracking Index
600
V
Cond.; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
18.0
µm/m-°C
Dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow
110
µm/m-°C
Dry; ISO 11359-1/-2
Melting Point
255
°C
10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
245
°C
Dry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
225
°C
Dry; ISO 75-1/-2
Vicat Softening Point
195
°C
50°C/h 50N; Dry; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
IEC 60695-11-10
HB
@Thickness 3.20 mm
IEC 60695-11-10
Processing Properties
Original Value
Comments
Melt Temperature
280
°C
Injection Molding; ISO 294
Mold Temperature
70.0
°C
Injection Molding; ISO 10724
Descriptive Properties
Form as Delivered
Pellets
Heat Stabilized
Yes
Light Stabilized
Yes
Moisture Sensitive
Yes
Processing Methods
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
CENTROPLAST CENTROMID 6.6 GF 30 Polyamide 6.6 30% glass fiber
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Conditioned, 50% Glass Filled
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled
PARKG466 / 24510
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.