Z-ULTRAT Plus is a material which combines high impact resistance and improved adhesion between individual layers in models. Its qualities provide enhanced durability of 3D printed items, allowing you to create complex mechanisms and strong end-use parts. Z-ULTRAT Plus is based on ABS and therefore is a perfect alternative for this widely known and used by the industry thermoplastic. This material becomes the best choice for many areas, including automotive or manufacturing, where prototypes require high tolerance during impact tests.Information provided by Zortrax |