MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huntsman Rexell® H2103 Injection Molding LLDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Linear-low medium density homopolymer, injection molding, FDA compliant.

Features: Good ESCR, low taste and order.

Applications: Containers, closures, and ideal for blends and non-carbonated beverage caps.

FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2.a

Information provided by Huntsman Corporation

Key Words: Linear Low Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D1505
Viscosity  66 cP
@Shear Rate 5000 1/s,
Temperature 230 °C
66 cP
@Shear Rate 5000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
 144 cP
@Shear Rate 1000 1/s,
Temperature 230 °C
144 cP
@Shear Rate 1000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
 228 cP
@Shear Rate 300 1/s,
Temperature 230 °C
228 cP
@Shear Rate 300 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
Melt Flow 10.7 g/10 min10.7 g/10 minMelt Flow Ratio (I10/I2) is 7.7; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
Tensile Strength, Ultimate 11.0 MPa1600 psiASTM D638
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 200 %200 %ASTM D638
Modulus of Elasticity 0.938 GPa136 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 117 °C243 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUP69 / 47878

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.