MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Avient Elastamax™ XL-0257-2 TPU-Based Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color: Grey.

Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 212 g/10 min
@Load 2.16 kg,
Temperature 210 °C
212 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 51515 sec. delay; ASTM D2240
Tensile Strength, Ultimate 15.9 MPa2310 psi10 in/min; ASTM D412
Elongation at Break 212 %212 %10 in/min; ASTM D412
50% Modulus 11.45 MPa
@Strain 50 %
11.45 MPa
@Strain 50 %
10 in/min; ASTM D412
100% Modulus 11.93 MPa
@Strain 100 %
1730 psi
@Strain 100 %
ISO 37
Izod Impact, Notched 3.74 J/cm
@Thickness 3.17 mm
7.01 ft-lb/in
@Thickness 0.125 in
ASTM D256

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® DP 7-1158 Urethane Thermoplastic Elastomer
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU)
Covestro Texin® 950 Urethane Thermoplastic Elastomer
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU

PHG884 / 47004

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.