MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huber Zerogen® 100 SP Magnesium Hydroxide
Categories: Ceramic; Oxide; Magnesium Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Zerogen® magnesium hydroxide products provide excellent fire retarding and smoke suppression performance for the thermoplastic and elastomeric compounds. The Zerogen 100 products are characterized by higher chemical purity compared to Zerogen 50 products and therefore provide further enhanced performance in compound applications where superior electrical properties are needed, e.g. cable primary insulation materials. Zerogen 100 SP is an ultrafine particle size; low surface area magnesium hydroxide with vinyl silane treatment designed to provide excellent compounding rheology, high-quality powder dispersion and enhanced compound mechanical properties in such polymers as polyolefins, EPR/EPDM and other elastomers.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.40 g/cc2.40 g/cc
Particle Size 0.80 µm0.80 µmMedian Particle Size
Particle Mesh Size 325 Mesh325 Mesh<0.5% Residue
Specific Surface Area 5.0 m²/g5.0 m²/gBET
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca <= 0.020 %<= 0.020 %
Free Water <= 0.10 %
@Temperature 105 °C
<= 0.10 %
@Temperature 221 °F
Free
Iron, Fe <= 0.0050 %<= 0.0050 %
Loss on Ignition(%) >= 31 %
@Temperature 1200 °C
>= 31 %
@Temperature 2190 °F
 
Descriptive Properties
ColorWhite
Content<0.02%Chloride
 >99.5%Mg(OH)2
FunctionalityLow Moisture Pick-Up
 Smoke Suppression
Functionality: Electrical PropertiesWet-Rated Insulation 90°C
Functionality: Mechanical hardnessImproved Physical Properties
Market/Application: E & E, InfrastructureElectrical Switches, Connectors
Market/Application: Wire and CableWire & Cable Insulation - Halogen-Free

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER799 / 300905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.