MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Goodfellow Carbon-Carbon Composite
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: Carbon Fiber - Carbon Matrix

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 - 1.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break <= 10.0 MPaTransverse
 40.0 - 70.0 MPaLongitudinal
Tensile Modulus 20.0 - 30.0 GPaParallel to Plane
Flexural Strength 80.0 - 200 MPaParallel to Plane
Flexural Modulus 10.0 - 20.0 GPaParallel to Plane
Compressive Strength 60.0 - 150 MPaPerpendicular to Plane
 120 - 200 MPaParallel to Plane
Shear Strength 20.0 - 30.0 MPain Plane
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00300 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 1.50 µm/m-°C
@Temperature 20.0 - 1000 °C
CTE, linear, Transverse to Flow 6.00 µm/m-°C
@Temperature 20.0 - 1000 °C
 6.00 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 50.0 - 100 W/m-KPerpendicular to Plane
 250 - 300 W/m-KParallel to Plane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlisle 201HD Carbon-Carbon Composite
Carlisle 201HL Carbon-Carbon Composite
Carlisle 201LD Carbon-Carbon Composite
Carlisle 201LL Carbon-Carbon Composite
Solvay Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

PGOODF116 / 42271

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.