System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
ExxonMobil Paxon™ AA50-002 Blow Molding Resin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Blow Molding Grade
Material Notes:
AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.
Information provided by ExxonMobil Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.950
g/cc
ASTM D4883
ESCR 100% Igepal®
80
hour
ASTM D1693 Condition B
Melt Flow
0.20
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
2300
psi
ASTM D638
Tensile Strength, Yield
3900
psi
ASTM D638
Elongation at Break
900 %
ASTM D638
Elongation at Yield
9.0 %
ASTM D638
Tensile Modulus
300000
psi
ASTM D638
Flexural Modulus
185000
psi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength
90.0
ft-lb/in²
ASTM D1822
Thermal Properties
Original Value
Comments
CTE, linear
120
µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
68.0
°C
ASTM D648
Vicat Softening Point
255
°F
ASTM D1525
Brittleness Temperature
<=
-76.0
°F
ASTM D746
Processing Properties
Original Value
Comments
Melt Temperature
375
°F
Descriptive Properties
Features
Thermal Stabilizer
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
ExxonMobil HD 9856B Blow Molding Resin
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
Borealis BL0521 High Density Polyethylene
Celanese GUR® 4170 PE-UHMW, Unfilled
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade
PEXB090 / 37395
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.