MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB845MO can be steam-sterilized at 250°F for 20 minutes because of its high heat distortion temperature (HDT).

Bormed RB845MO is designed for pharmaceutical and diagnostic packaging, bottles for parentheral solutions, containers for injectable solutions, and containers for fine chemicals.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3800 psiAt 50 mm/min; ASTM D638
Elongation at Yield 13 %At 50 mm/min; ASTM D638
Tensile Modulus 1.00 GPaAt 1 mm/min; ASTM D638
Charpy Impact, Notched 0.700 J/cm²ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications
Borealis Bormed™ HD850MO Polypropylene Copolymer for Healthcare Applications
Borealis Bormed™ HF855MO Polypropylene Homopolymer for Medical Applications
Borealis RB307MO Polypropylene Random Copolymer
Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications

PBOREA080 / 27387

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.