1020 steel responds well to cold work and heat treating. Weldability is fair. Applications: Shafts, lightly stressed gears, hard wearing surfaces, pins, chains and case hardened parts where core strength is not critical. 1020 is suitable for case hardened parts where core strength is not critical. |
UNS G10200, AMS 5032, AMS 5045, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A29, A108, A510, A512, A513, A519, A544, A575 M10120, A576, A635, A659, A827, A830, BS 970 040A20, 050A20 (En2C), 050A20 (En2D), 060A20, BS 970 Part 1 070M20, DEF STAN95-1-1 C1020, SAE J412, SAE J414, DIN 1.0402, AFNOR CC 20, UNI C 20, SS14 1450 (Sweden), SAE J403 |