MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MOL Group TIPELIN 3110J HDPE, Injection molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Description: TIPELIN 3110J is a copolymer polyethylene (butene-1 comonomer), intended for injection molding and compression molding of general purpose products. It offers good organoleptic properties, environmental stress crack resistance and improved long-term color stability. The grade contains antioxidant, acid scavenger and slip agent.

Applications: TIPELIN 3110J is recommended for caps and closures for carbonated soft drinks, engineering and technical parts.

(1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements carried out on standard injection molded specimens (ISO 294-1) conditioned at room temperature (ISO 291).

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³1; ISO 1183-1
ESCR 100% Igepal® 20 hour20 hour1, CO-630; ASTM D 1693
Oxidative Induction Time (OIT) 65 min
@Temperature 200 °C
65 min
@Temperature 392 °F
EN 728
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62622; ISO 868
Tensile Strength at Break 25.0 MPa3630 psiISO 527-1,2
Tensile Strength, Yield 23.0 MPa3340 psi2; ISO 527-1,2
Elongation at Break 800 %800 %ISO 527-1,2
Elongation at Yield 12 %12 %2; ISO 527-1,2
Flexural Modulus 1.00 GPa145 ksi2; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²2; ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 127 °C261 °FISO 306/A 120
Shrinkage, MD 1.8 %1.8 %2; ISO 294-4
Shrinkage, TD 3.0 %3.0 %2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 200 °C338 - 392 °Fcompression molding
 210 - 250 °C410 - 482 °Finjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG042 / 297208

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.