MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger HYDEX® 4101 UD Blue Ultra Detectable Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: HYDEX® 4101 UD Blue is an Ultra Detectable PBT designed specifically for applications in the food industry.

Main features:

  • resistant to cleaning agents
  • food grade blue
  • good chemical resistance
  • good dimensional stability
  • good impact strength
  • metal detectable
  • x-ray opaque
Target Industries:
  • food processing
  • food engineering
  • conveyor technology
  • packaging and paper machinery

Information provided by Ensinger Special Polymers, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.59 g/cc1.59 g/ccASTM D790
Moisture Absorption 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9292ASTM D785
Tensile Strength 64.12 MPa9300 psiASTM D638
Elongation at Break 3.53 %3.53 %ASTM D638
Tensile Modulus 3.79 GPa550 ksiASTM D638
Flexural Strength 105.1 MPa15250 psiASTM D790
Flexural Modulus 3.835 GPa556.2 ksiASTM D790
Compressive Yield Strength 22.1 MPa
@Strain 1 %
3200 psi
@Strain 1 %
ASTM D695
Compressive Strength 94.87 MPa
@Strain 10 %
13760 psi
@Strain 10 %
ASTM D695
Compressive Modulus 2.388 GPa346.4 ksiASTM D695
Izod Impact, Notched 0.310 J/cm0.580 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.9 µm/m-°C40.5 µin/in-°FASTM D696
Melting Point 225 °C437 °FASTM D3418
Maximum Service Temperature, Air 105 °C221 °FLong Term; UL746B
Deflection Temperature at 0.46 MPa (66 psi) 201 °C393 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger HYDEX® 4101 Polybutylene Terephthalate (PBT)
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
Ensinger HYDLAR® Z Nylon, Pultruded Aramid Fiber Reinforced (PA)
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66)

PENSIN036d / 193514

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.