Glass Fiber Reinforced grades-10% glass fiber, flame resistant grade, Non-Bromine / non-phosphorus. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Filter / reinforcement: Glass fiber, 10% filler by weight. Features: Bromine Free, Creep resistant, flame resistant, High Rigidity. Uses: Camera Applications, Electrical parts, industrial applications. Forms: pellets. Processing Method: Injection Molding.Information provided by Teijin Chemicals Ltd. |