MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Abatron AboCast/AboCure 8109-10
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.

Processing: 100% solids; 100/130 ratio; Potlife: 6-8 days/20°C (68°F); 1-2 days 40°C (105°F), 10-15 hours at 60°C (140°F); cures im: 8 h/80°C (175°F), 6 h/100°C (212°F), 4 h/120°C (250°F); mix thoroughly at RT, heat to desired viscosity, apply to clean, dry surface.

Applications: Impregnating and potting.

Key Words: impregnating, composites, potting
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
Water Absorption 0.20 - 0.35 %(60x10X4 mm bar) after 10 days at 20°C (77°F)
 0.30 - 0.45 %(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 3500 - 6500 cP
 30 - 60 cP
@Temperature 60.0 °C
 350 - 650 cP
@Temperature 40.0 °C
Vapor Pressure 1.00 torr
@Temperature 180 °C
AboCast
 1.00 torr
@Temperature 100 °C
AboCure
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 55.15 MPa
Modulus of Elasticity 2.068 GPa
Flexural Yield Strength 86.18 MPa
Compressive Yield Strength 89.63 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.50e+16 ohm-cm
Dielectric Constant 2.5 - 3.0
@Frequency 1000 Hz
 2.6 - 3.1
@Frequency 1e+6 Hz
 2.7 - 3.2
@Frequency 50 Hz
Dielectric Strength 300 - 400 kV/in
@Thickness 3.17 mm
Short time value
Dissipation Factor 0.0030 - 0.0060
@Frequency 50 Hz
 0.0050 - 0.0070
@Frequency 1000 Hz
 0.010 - 0.015
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 95.0 - 105 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 70.0 °CDeflection temperature; load unknown.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 25.0 °C
Pot Life 600 - 900 min
@Temperature 60.0 °C
 1440 - 2880 min
@Temperature 40.0 °C
 8640 - 11520 min
@Temperature 20.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Applied Composites 120 Polyester SMC
Applied Composites 150 Polyester SMC
Applied Composites 175 Vinylester SMC
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Applied Composites 8033 Polyester SMC

PABEY1 / 22024

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.