MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Universal Wire Works Hastelloy X (AMS 5798) Filler Metal
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Hastelloy Alloy X welding wire can be used with the gas tungsten arc, gas metal arc and plasma welding processes. Alloy X is used extensively in high temperature applications including engine tailpipes, turbine blades, afterburner components, nozzle vanes, cabin heaters and combustion liners.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 0.010 %<= 0.010 %
Carbon, C 0.10 %0.10 %
Chromium, Cr 22 %22 %
Cobalt, Co 1.5 %1.5 %
Iron, Fe 19 %19 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 9.0 %9.0 %
Nickel, Ni >= 45.7 %>= 45.7 %As Remainder
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W 0.60 %0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes Hastelloy® X alloy, sheet
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Haynes Hastelloy® B-3® alloy, 0% cold work
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy
Carlson C 625 Nickel-Chromium-Molybdenum Alloy

NUWW308 / 19740

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.