MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Matexcel ANT-0052 Transparent Heat-curing Antimicrobial Hardened and Wear-resistant Protective Coating for Metal
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: This coating forms a uniformly distributed coating on the metal surface by hybridizing nano-inorganic oxides and organic polymers. It can effectively combine with the metal substrate, improve the adhesion of the coating, to form a dense protective film. It can also effectively improve the hardness and wear resistance of the coating, greatly improve the antibacterial and mildew resistance, and effectively protect the metal products from corrosion. It also functions as hydrophobic, oleophobic, stain-resistant and sweat-resistant, etc. 1. Excellent antibacterial performance, antibacterial rate =99.99% (Staphylococcus aureus, E. coli, mold, etc.); 2. Good abrasion resistance; excellent adhesion, the cross frame adhesion reaches level 0; 3. Strong weather resistance, not afraid of temperature changes such as sun, rain, wind, summer heat, cold weather, etc. It will not produce yellowing when exposed to the outdoors for a long time; 4. The surface of the paint film is smooth and full; 5. The paint film has good flexibility and high hardness; 6. Colorless and transparent, will not change the color and appearance of the original substrate.

Application: It is suitable for hardening, abrasion resistance, antibacterial and mildew protection treatment of various metal materials, such as various aluminum profiles, stainless steel, nickel-plated zinc alloy and nickel-plated copper alloy.

Morphology: Light yellow transparent liquid

Uses: Before painting, the metal surface must be cleaned and dried with a solvent or detergent to remove all oil stains, grease or other contaminants. According to the different conditions of the shape, size and surface state of the metal material, choose spraying and other processes for painting. It is recommended to sample test before construction. First spray the primer coating on the metal surface, the primer coating is self-drying type, and let it dry after standing for top coating. Then spray antibacterial and antifungal paint on the basis of primer, then put it for 3-5 minutes, and then cure at 110 °C for 40 minutes. 1. Sealed and stored in a cool place with clear labels to prevent misuse and misuse; 2. Keep away from fire and heat sources, and keep it out of the reach of children; 3. The workplace should have good ventilation conditions, and fireworks are strictly prohibited; 4. It is recommended that operators wear work protective clothing, chemical protective gloves, and goggles; 5. Prohibit entrance, avoid contact with eyes and skin. In case of splash into eyes, immediately rinse with plenty of water and seek medical advice.

Key Words: Transparent Heat-curing Antimicrobial Hardened and Wear-resistant Protective Coating for Metal
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 7.0
Viscosity 10 cP
Storage Temperature 20.0 °CStored in a cool, dry place, avoid direct sunlight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK1485 / 300116

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.