MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik KANTHAL 100% Nickel Resistance Strip
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: 100% Nickel is used as an intermediate layer in bimetals.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 400 MPa
Tensile Strength, Yield 160 MPa
@Strain 0.2 %
Elongation at Break 35 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000900 ohm-cm
 0.00000900 ohm-cm
@Temperature 20.0 °C
 0.0000126 ohm-cm
@Temperature 100 °C
 0.0000187 ohm-cm
@Temperature 200 °C
 0.0000267 ohm-cm
@Temperature 300 °C
 0.0000343 ohm-cm
@Temperature 400 °C
 0.0000380 ohm-cm
@Temperature 500 °C
 0.0000415 ohm-cm
@Temperature 600 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.3 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.480 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 70.0 W/m-K
@Temperature 100 °C
Melting Point 1450 °C
Maximum Service Temperature, Air 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe <= 0.25 %
Manganese, Mn <= 0.30 %
Nickel, Ni >= 99.2 %
Silicon, Si <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Kanthal Nikrothal 42 Resistance heating wire and resistance wire
Sandvik Kanthal AF Resistance Strip
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems Inconel 601 Washers and Studs
Kanthal® 70 Resistor Material
Kanthal® 52 Nickel-Iron Resistor Alloy

NSANDV059 / 18953

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.