MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

American Elements Gadolinium Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Gadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 75 - 90 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Gadolinium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for gadolinium nanocrystals has focused on use in magnetic resonance imaging (MRI) by targeting coated gadolinium particles at tumors in an attempt to detect or label early stage cancer, particularly breast cancer, for Neutron Capture Therapy and for MRI Contrast Enhancement, as a dopant in glass and for their potential electrical, dielectric, magnetic, optical, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, nanofiber and textiles and in alloy and catalyst applications.

Key Words: Formula: Gd; CAS Number: 7440-54-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.901 g/cc0.2854 lb/in³
Particle Size 0.010 - 0.045 µm0.010 - 0.045 µm
 0.075 - 0.090 µm0.075 - 0.090 µm
Specific Surface Area 5.0 - 10 m²/g5.0 - 10 m²/g
 30 - 50 m²/g30 - 50 m²/g
Molecular Weight 157.25 g/mol157.25 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1312 °C2394 °F
Boiling Point 3250 °C5880 °F
 
Descriptive Properties
AppearanceBlack
StabilityModerately reactive in air

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EJAMER33 / 5516

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.