MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Domo TECHNYL® A 222 Black 1N PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .

Available in: Europe

Product Applications: TECHNYL A 222 offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity .These performances are associated with excellent dimensional stability and good rigidity of molded parts. This grade is used for connector parts in electrical and automotive industries. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183/A
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
1.1 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0093 cm/cm0.0093 in/inIsotropy
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/in
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psiISO 527 Type 1A
Tensile Strength, Yield 95.0 MPa13800 psiISO 527 type 1 A
Elongation at Break 20 %20 %ISO 527 Type 1A
Elongation at Yield 7.0 %7.0 %ISO 527 type 1 A
Tensile Modulus 3.20 GPa464 ksiISO 527 Type 1A
Flexural Modulus 3.10 GPa450 ksiISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 2.92.9IEC 60250
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243
Dissipation Factor 0.0300.030IEC 60250
Comparative Tracking Index 450 V450 VSolution B; IEC 60112
 575 V575 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FISO 75/Af
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
Oxygen Index 26 %26 %ISO 4589
Glow Wire Flammability Index 700 °C1290 °FISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-285°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 222 Black 1N PA66, Conditioned
Domo Technyl® A 246M Nylon 66, Impact Grade, EH50
Domo Technyl® A 246M Nylon 66, Impact Grade, EH0

PRHOD687 / 137918

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.