System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Celanese Zytel® 70G30HSLR BK099 PA66-GF30
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 30% Glass Fiber Filled
Material Notes:
30% Glass Reinforced, Heat Stabilized, Hydrolysis Resistant, Polyamide 66
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.37
g/cc
DAM; ISO 1183
Water Absorption
1.3 %
@Time 86400 sec
Immersion; DAM; Sim. to ISO 62
6.0 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption
1.90 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity
190000
cP
@Shear Rate 1000 1/s,
Temperature 280 °C
Melt; ISO 11443
Viscosity Number
150
cm³/g
acid sulfuric 96%; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow
0.0030
cm/cm
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.010
cm/cm
DAM; ISO 294-4, 2577
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
88
50% RH; ISO 2039-2
104
DAM; ISO 2039-2
Hardness, Rockwell R
117
50% RH; ISO 2039-2
124
DAM; ISO 2039-2
Ball Indentation Hardness
185
MPa
H 961/30; 50% RH; ISO 2039-1
270
MPa
H 961/30; DAM; ISO 2039-1
Tensile Strength at Break
130
MPa
50% RH; ISO 527-1/-2
200
MPa
DAM; ISO 527-1/-2
Elongation at Break
3.0 %
DAM; ISO 527-1/-2
5.0 %
50% RH; ISO 527-1/-2
Tensile Modulus
7000
MPa
50% RH; ISO 527-1/-2
10000
MPa
DAM; ISO 527-1/-2
Flexural Strength
200
MPa
DS; 50% RH; ISO 178
280
MPa
DS; DAM; ISO 178
Flexural Modulus
6500
MPa
DS; 50% RH; ISO 178
9000
MPa
DS; DAM; ISO 178
Poissons Ratio
0.34
DAM
0.35
50% RH
Izod Impact, Notched (ISO)
10.0
kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
10.0
kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
10.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
12.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched
65.0
kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
70.0
kJ/m²
@Temperature -30.0 °C
DS; 50% RH; ISO 179/1eU
70.0
kJ/m²
@Temperature -30.0 °C
DS; DAM; ISO 179/1eU
70.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
80.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched
9.00
kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
9.00
kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
9.00
kJ/m²
@Temperature -30.0 °C
DS; 50% RH; ISO 179/1eA
9.00
kJ/m²
@Temperature -30.0 °C
DS; DAM; ISO 179/1eA
12.0
kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
15.0
kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Impact Test
5.00
J
@Thickness 2.00 mm
Multiaxial Impact, Total Energy; 4.5m/s; DAM; ISO 6603-2
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+11
ohm-cm
DS; 50% RH; IEC 62631-3-1
>=
1.00e+15
ohm-cm
DS; DAM; IEC 62631-3-1
Surface Resistance
1.00e+12
ohm
DS; 50% RH; IEC 62631-3-2
Dielectric Strength
32.0
kV/mm
50% RH; IEC 60243-1
38.0
kV/mm
DAM; IEC 60243-1
Comparative Tracking Index
400
V
DAM; IEC 60112
400
-
599
V
PLC 1; DAM; UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
22.0
µm/m-°C
DAM; ISO 11359-1/-2
13.0
µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
26.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow
80.0
µm/m-°C
DAM; ISO 11359-1/-2
70.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
130
µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Specific Heat Capacity
2.29
J/g-°C
@Temperature 295 °C
Melt
Melting Point
262
°C
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
261
°C
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)
253
°C
DAM; ISO 75-1/-2
Glass Transition Temp, Tg
20.0
°C
10°C/min; 50% RH; ISO 11357-1/-2
75.0
°C
10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94
HB
@Thickness 0.750 mm
DAM; IEC 60695-11-10
HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread
37.0
mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index
24 %
DAM; ISO 4589-1/-2
Processing Properties
Original Value
Comments
Melt Temperature
295
°C
Optimum, Injection
285
-
305
°C
Range, Injection
Mold Temperature
70.0
-
120
°C
Injection
100
°C
Optimum, Injection
Ejection Temperature
210
°C
Injection
Drying Temperature
80.0
°C
Injection
Dry Time
2.00
-
4.00
hour
Injection, Dehumidified Dryer
Moisture Content
<= 0.20 %
Injection
Hold Pressure
50.0
-
100
MPa
Range, Injection
Descriptive Properties
Additives
Release agent
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
ISO designation
ISO 16396-PA66,GF30,M1CGHRW,S14-100
Max. screw tangential speed (m/s)
0.2
Injection
Odor Class
5
VDA 270
Part Marking Code
>PA66-GF30<
ISO 11469
Polymer
PA66-GF30
Processing Hold Pressure Time (s/mm)
3
Injection
Resin Identification
PA66-GF30
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 70G30HSL BK039B PA66-GF30
DuPont Mobility and Materials Zytel® 70G30HSL NC010 PA66-GF30
Celanese Zytel® 70G30HSLR NC010 PA66-GF30
Celanese Zytel® 70G30L NC010 PA66-GF30
Celanese Zytel® 103HSL NC010 PA66
PDSX5325 / 197965
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.