MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

High-Strength Yellow Brass, UNS C86500, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Shrinkage in Solidification, Drossing; Medium – Fluidity; Low – Casting Yield, Effect of Section Size, Gassing

Fabrication Properties: Fair Suitability – Soldering, Brazing; Poor Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical uses: Weld Guns; Brackets; Electrical Hardware; Electrical Hardware; Forming Dies for Wood Pulp Industry; Frames; Gears; Hooks; Lever Arms; Machinery; Machinery Parts (Substituted for Steel and Malleable Iron); Machinery Parts requiring High Strength; Pressing Dies for Wood Pulp; Struts; Wear Rings for Pressing Dies for Wood Pulp Industry; Boat Parts; Clamps; Covers for Marine Hardware; Propellers for salt and fresh water; Rudders

Applicable Specifications: As Centrifugal Cast - Castings ASTM B271/B271M, Castings AMS 4860, Castings SAE J462, Castings SAE J461; As Continuous Cast – Castings ASTM B505/B505M; As Die Cast – Castings ASTM B176; As Sand Cast – Castings AMS 4860, SAE J462, Castings ASTM B584, Castings SAE J461, Castings ASTM B763/B763M; Ingot - ASTM B30, FEDERAL QQ-C-523

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.33 g/cc0.301 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 448 MPa>= 65000 psifor Standard
Tensile Strength, Yield >= 172 MPa>= 25000 psifor Standard, 0.5% Ext
Elongation at Break >= 20 %>= 20 %for Standard
Tensile Modulus 103 GPa15000 ksi
Machinability 26 %26 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000780 ohm-cm0.00000780 ohm-cm22% IACS
Magnetic Permeability 1.091.09Field Strength 16 kA/m
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 100 °C
11.3 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 7.15 W/m-K49.6 BTU-in/hr-ft²-°F
Melting Point 861.7 - 880.0 °C1583 - 1616 °F
Solidus 861.7 °C1583 °F
Liquidus 880.0 °C1616 °F
Shrinkage 2.08 %2.08 %Patternmaker's Shrinkage (4/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.50 - 1.5 %0.50 - 1.5 %
Copper, Cu 55 - 60 %55 - 60 %
Iron, Fe 0.40 - 2.0 %0.40 - 2.0 %
Lead, Pb <= 0.40 %<= 0.40 %
Manganese, Mn 0.10 - 1.5 %0.10 - 1.5 %
Nickel, Ni <= 1.0 %<= 1.0 %
Tin, Sn <= 1.0 %<= 1.0 %
Zinc, Zn 36 - 42 %36 - 42 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC86500x1 / 293170

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.