MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 20% Glass Fiber Reinforced

Material Notes: Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire test up to 960°C.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Moisture Absorption at Equilibrium 2.0 - 2.4 %23°C; 50% RH; ISO 62
Viscosity Measurement 130ISO 307
Melt Flow 157.2 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 45.0 MPa50 mm/min; ISO 527-1/-2
Elongation at Yield 6.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 2.70 GPaISO 527-1/-2
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 550 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 °CDIN 53765
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °CInjection-molding/Extrusion
Mold Temperature 60.0 - 80.0 °CInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Dry)
BASF Ultramid® C3U10 PA6/66 FR (Dry)
BASF Ultramid® 8253 PA6 (Conditioned)
Envalior Akulon® Ultraflow K-FG6 PA6-GF30, Dry, 30% Glass Filled, High Flow
Envalior Akulon® Ultraflow K-FPG8 PA6-I-GF40, Dry, 40% Glass Filled, High Flow

PBASG0331 / 131964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.