MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SACO AEI PEXIDAN® HF X/T Moisture-curable Low Smoke Zero-Halogen (LSZH) insulation compound
Categories: Polymer; Thermoset

Material Notes: Moisture-curable Low Smoke Zero-Halogen (LSZH) insulation compound for low-voltage building wire applications (UL styles XHHW-2, RHW-2, RHH, and SIS).

PEXIDAN® HF X/T is a low smoke halogen free flame retardant 90°C wet-rated XL-insulation system curable by moisture. It consists of a silane pre-grafted base compound SX651 and a catalyst masterbatch CM540U. Mixed and extruded in the proper proportions (95:5), the two components result in a material that is crosslinkable by exposure to 90°C hot water. PEXIDAN® HF X/T is REACH and RoHS-compliant and is UL 2885 certified to bear the Halogen Free “HF” designation. PEXIDAN® HF X/T is UL-bulletinized and wire made with this insulation system may be marked as Oil Resistant “PR I” and “PR II”, Gas & Oil Resistant “GR I” and “GR II”, “-40C” and “SUNRES” in all colors. This compound will meet a 105°C dry rating.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
pH 5.725.72Combustion Gas; IEC 60754-2
Deformation <= 15 %<= 15 %UL 1581 / UL 2556
Storage Temperature <= 29.4 °C<= 85.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 14.4 MPa2090 psiUL 1581 / UL 2556
 12.8 MPa
@Temperature 75.0 °C
1860 psi
@Temperature 167 °F
After 60 days oil (OILRES II); UL 1581 / UL 2556
 12.46 MPa
@Temperature 100 °C,
Time 346000 sec
1807 psi
@Temperature 212 °F,
Time 96.0 hour
Oil (OILRES I); UL 1581 / UL 2556
 17.0 MPa
@Temperature 121 °C,
Time 605000 sec
2470 psi
@Temperature 250 °F,
Time 168 hour
thermal ageing; UL 1581 / UL 2556
Tensile Strength, Yield 14.58 MPa2115 psiUL 1581 / UL 2556
 14.58 MPa2115 psiUL 1581 / UL 2556
Elongation at Break 270 %270 %UL 1581 / UL 2556
 270 %
@Temperature 75.0 °C
270 %
@Temperature 167 °F
After 60 days oil (OILRES II); UL 1581 / UL 2556
 <= 35 %
@Temperature 150 °C,
Time 900 sec
<= 35 %
@Temperature 302 °F,
Time 0.250 hour
Hot, 0.2 N/mm2 load; SACO AEI DWI-QA-4007 based on ICEA T-28-562
 235 %
@Temperature 100 °C,
Time 346000 sec
235 %
@Temperature 212 °F,
Time 96.0 hour
Oil (OILRES I); UL 1581 / UL 2556
 240 %
@Temperature 121 °C,
Time 605000 sec
240 %
@Temperature 250 °F,
Time 168 hour
thermal ageing; UL 1581 / UL 2556
Crush Resistance >= 635 kg>= 1400 lb (mass)UL 1581 / UL 2556
 
Electrical PropertiesMetricEnglishComments
Insulation Resistivity  33.5 Megaohm/1000 m
@Temperature 90.0 °C
110 Megaohm/1000 ft
@Temperature 194 °F
After 12 weeks; UL 1581 / UL 2556
 427 Megaohm/1000 m
@Temperature 90.0 °C
1400 Megaohm/1000 ft
@Temperature 194 °F
Initial; UL 1581 / UL 2556
 2740 Megaohm/1000 m
@Temperature 15.0 °C
9000 Megaohm/1000 ft
@Temperature 59.0 °F
UL 1581 / UL 2556
Dielectric Constant  2.98
@Frequency 1e+8 Hz
2.98
@Frequency 1e+8 Hz
ASTM D150
 3.31
@Frequency 5.00e+8 Hz
3.31
@Frequency 5.00e+8 Hz
ASTM D150
Dielectric Breakdown >= 31590 V>= 31590 VRetention after glancing impact; UL 1581 / UL 2556
 >= 39000 V>= 39000 Vinitial; UL 1581 / UL 2556
Dissipation Factor  0.0027
@Frequency 1e+8 Hz
0.0027
@Frequency 1e+8 Hz
ASTM D150
 0.0052
@Frequency 5.00e+8 Hz
0.0052
@Frequency 5.00e+8 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Smoke Density <= 50<= 50Flaming, corrected; ASTM E662
 <= 70<= 70Non-flaming, corrected; ASTM E662
 <= 1.0
@Time 240 sec
<= 1.0
@Time 0.0667 hour
Flaming; ASTM E662
 <= 2.0
@Time 240 sec
<= 2.0
@Time 0.0667 hour
Non-flaming; ASTM E662
Oxygen Index 34 %34 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 154 - 171 °C309 - 340 °Fbarrel zones
Die Temperature 179 °C354 °F
Head Temperature 177 °C351 °F
 
Descriptive Properties
Conductivity0.128 µS/mmCombustion Gas, IEC 60754-2
Degree of Crosslinking77%ASTM D2765
Flame ResistancePasses FT2UL 1581 / UL 2556
 Passes VW-1UL 1581 / UL 2556

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSACO008 / 249375

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.