MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® 60CF6 Nylon 6, 20% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Notes: 60CF6 is a 30% carbon fiber grade of nylon 6. It offers outstanding strength and stiffness-coupled with low density and improved electrical conductivity of molded parts. It is suitable for applications such as bearings and mechanical parts.

Availability: Europe

Fillers/Reinforcement: Carbon Fiber, 30% Filler by Weight

Features: High Stiffness; High Strength; Low Density

Uses: Bearings; Machine/Mechanical Parts

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.1 %2.1 %50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 210 MPa30500 psiISO 527-2
Elongation at Break 3.5 %3.5 %ISO 527-2
Tensile Modulus 17.0 GPa2470 ksiISO 527-2
Flexural Strength 300 MPa43500 psiISO 178
Flexural Modulus 18.5 GPa2680 ksiISO 178
Izod Impact, Notched (ISO) 5.04 kJ/m²2.40 ft-lb/in²ISO 180/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 200 °C>= 392 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 280 °C482 - 536 °F
Middle Barrel Temperature 250 - 280 °C482 - 536 °F
Front Barrel Temperature 250 - 280 °C482 - 536 °F
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0373 / 236864

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.