MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik REVOCOROS® AL 200 Corrosion Inhibitor
Categories: Other Engineering Material

Material Notes: Product description: REWOCOROS® AL 200 is a lauryl polyglycol ether based phosphoric acid ester.

Application: REWOCOROS® AL 200 is used as a corrosion inhibitor for aluminum and steel. Furthermore, it can be used as an efficient extreme pressure (EP) and anti-wear (AW) additive for water based metalworking fluids. Co-emulsifying properties have often been observed. It improves lubricity in neat rolling and drawing oils.

Properties/Benefits: REWOCOROS® AL 200 provides excellent corrosion inhibition on aluminum and in combination with amines also on steel even in low alkaline systems (pH 8).

  • REWOCOROS® AL 200 provides excellent EP/AW properties in water based metalworking fluids.
  • REWOCOROS® AL 200 is 73 % readily bio-degradable (OECD 301 E).

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 1.0 - 3.01.0 - 3.0
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 140 - 160140 - 160[mg KOH/g]
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.5 %<= 1.5 %
 
Descriptive Properties
Coloryellow, clear to slightly turbid, liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TAGAT® TO V Emulsifier
Evonik REVOCOROS® AC 100 US Corrosion Inhibitor
Evonik REVOCOROS® AC 144 Corrosion Inhibitor
Solvay GEROPON® HW 15 Surfactant
Solvay RHODAQUAT® M-242B/99 Surfactant

PEVONIM137 / 197341

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.