MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adsyl C 39 F Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adsyl 5 C 39 F is an advanced polyolefin, selected by customers for use as a sealing or metalized layer in coextruded film applications. This grade features a very low seal initiation temperature. It contains anti-block additives.

Availability: Africa-Middle East; Asia-Pacific; Europe; North America; South & Central America

Application: Barrier Film; Clarity Film; Food Packaging Film; Lamination Film; Sealants; Shrink Film; Specialty Film; Stationery Film

Market: Flexible Packaging

Processing Method: BOPP; Cast Film; Double Bubble

Attribute: High Transparency; Low Temperature Heat Sealability; Medium Antiblocking; Metallizeable; Terpolymer

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³Method A; ISO 1183-1
Melt Flow 5.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Heat Seal Strength Initiation Temperature 105 °C
@Thickness 0.0300 mm
221 °F
@Thickness 0.00118 in
 
Thermal PropertiesMetricEnglishComments
Melting Point 132 °C270 °FISO 11357-3
Vicat Softening Point 111 °C232 °FA/50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 0.600 %
@Thickness 1.27 mm
0.600 %
@Thickness 0.0500 in
ASTM D1003
Gloss 88.0 %88.0 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9021 / 323949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.