MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Thermx® CG033 PCT, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced

Material Notes: Thermx« CG033 is a 30% glass fiber reinforced polycyclohexylenedimethylene terephthalate for injection molding.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
Density of Compound 1.42 g/cc
Viscosity Test 85 cm³/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPa5mm/min; ISO 527-2/1A
Elongation at Break 2.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 8500 MPa50mm/min; ISO 527-2/1A
Flexural Strength 180 MPaISO 178
Flexural Modulus 8000 MPaISO 178
Charpy Impact Unnotched 50.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Strength 33.0 kV/mmIEC 60243-1
Comparative Tracking Index 560 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 85.0 µm/m-°CISO 11359-2
Specific Heat Capacity 1.47 J/g-°C
Thermal Conductivity 0.200 W/m-K
Melting Point 283 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 270 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 262 °CISO 75-1, -2
Glass Transition Temp, Tg 105 °CISO 11357-1,-2,-3
Flammability, UL94 HB
@Thickness 1.50 mm
Oxygen Index 29 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 120 °Ccavity
Melt Temperature 295 - 310 °C
Ejection Temperature 220 °C
Drying Temperature >= 95.0 °C
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Thermx® CG033 BK010T PCT
Celanese Thermx® CG023 NC010 PCT
Celanese Thermx® CG907 PCT, 30% Glass Reinforced

PHCQ463 / 178918

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.