MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Materion Copper Beryllium Alloy 165 Mill Hardened Strip AM (TM00) (UNS C17000)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloy 165 strip provides strength and conductivity close to Alloy 190 strip, with slightly less beryllium. This alloy features excellent stress relaxation resistance and high fatigue strength. Typical applications include high reliability spring contacts for switches and relays, battery contacts and automotive terminals.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 225 - 251225 - 251DPH Hardness
Tensile Strength, Ultimate 689 - 758 MPa100000 - 110000 psi
Tensile Strength, Yield 483 - 655 MPa
@Strain 0.200 %
70000 - 95000 psi
@Strain 0.200 %
Elongation at Break 18.0 - 30.0 %18.0 - 30.0 %
Modulus of Elasticity 131 GPa19000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000520 - 0.00000960 ohm-cm0.00000520 - 0.00000960 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.5 µm/m-°C9.70 µin/in-°F
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
Melting Point 870 °C1600 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.60 - 1.85 %1.60 - 1.85 %
Co + Ni >= 0.200 %>= 0.200 %
Co + Ni + Fe <= 0.600 %<= 0.600 %
Copper, Cu 97.55 - 98.2 %97.55 - 98.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB442va / 323468

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.