MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röchling SUSTARIN® C MDT POM/Metal Dectable Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes:
  • Metal detectable
  • Standard color: blue
  • High hardness rigidity
Product applications:
  • Materials handling industry
  • Mechanical engineering
  • Food processing industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³DIN EN ISO 183-1
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D2240
Elongation at Break 10 %10 %ASTM D638
Flexural Modulus 0.951 GPa138 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C12.0 µin/in-°FASTM D696
Melting Point 168 °C334 °F
Maximum Service Temperature, Air 85.0 °C185 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF NoNo
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9030 / 232733

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.