MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Thermal Ceramics K-25 Low Temperature Insulating Firebrick
Categories: Ceramic

Material Notes: Thermal Ceramics was first to introduce insulating firebrick (IFB) to the industry in the 1930’s. The IFB are manufactured with a unique slurry casting process which creates a network of microporosity which produces low thermal conductivity and good thermal shock characteristics. This process produces brick that are some of the most efficient insulators available in the market. The anorthite mineralogy (CaO, Al2O3, 2 SiO2) of these low temperature IFB gives them excellent strength at operating temperatures and resistance to corrosive alkali environments.

Features:

  • Extremely low “K” factors
  • Low densities
  • Low heat storage
  • Excellent strength at room and high temperatures
  • Excellent resistance to alkali attack
  • Excellent service in applications involving special atmospheres
  • Applications:

  • Backup insulation for carbon baking furnaces
  • Backup insulation in aluminum electrolytic cells
  • Electrical kilns for industrial and hobby use
  • Backup insulation for blast furnace stove linings
  • Linings for carbonizing furnaces
  • Forge furnace linings
  • Heat transfer linings
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.641 g/cc0.0232 lb/in³
    Deformation 0.10 %0.10 %at 10 psi; 1.5 hours at 2200°F; ASTM C16
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.000965 GPa0.140 ksiASTM C133
    Compressive Strength 1.52 MPa220 psiASTM C133
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.161 W/m-K
    @Temperature 260 °C
    1.12 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C201
     0.184 W/m-K
    @Temperature 538 °C
    1.28 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C201
     0.210 W/m-K
    @Temperature 816 °C
    1.46 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C201
     0.238 W/m-K
    @Temperature 1090 °C
    1.65 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    ASTM C201
    Melting Point 1540 °C2800 °F
    Maximum Service Temperature, Air 1370 °C2500 °F
    Shrinkage -0.100 %
    @Temperature 1340 °C,
    Time 86400 sec
    -0.100 %
    @Temperature 2450 °F,
    Time 24.0 hour
    ASTM C120
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 45 %45 %
    Alkalis 0.50 %0.50 %
    CaO 14.5 %14.5 %
    Fe2O3 0.20 %0.20 %
    MgO 0.20 %0.20 %
    SiO2 38 %38 %
    TiO2 1.6 %1.6 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM139 / 2459

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.