System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SCG Chemicals EL-Pro™ P401S Polypropylene Flat Yarn/Sheet
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Fiber Grade
Material Notes:
Key Characteristics:
Excellent mechanical properties
Recommended Applications:
Stretch tape for jumbo woven sheet
Monofilament for rope and sheet
Information provided by SCG Chemicals
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
0.910
g/cc
ASTM D1505
Environmental Stress Crack Resistance
>=
500
hour
@Temperature 50.0 °C
F50, 25% Igepal; ASTM D1693
Melt Flow
2.4
g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
85
ASTM D785
Tensile Strength at Break
25.0
MPa
ASTM D638
Tensile Strength, Yield
320
kg(f)/cm²
ASTM D638
Elongation at Break
650 %
ASTM D638
Flexural Modulus
14250
kg(f)/cm²
ASTM D790
Izod Impact, Notched
1.80
kg-cm/cm
@Temperature -20.0 °C
ASTM D256
2.80
kg-cm/cm
@Temperature 0.000 °C
ASTM D256
4.20
kg-cm/cm
@Temperature 23.0 °C
ASTM D256
Thermal Properties
Original Value
Comments
Melting Point
163
°C
ASTM D2117
Deflection Temperature at 0.46 MPa (66 psi)
110
°C
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
60.0
°C
ASTM D648
Vicat Softening Point
155
°C
ASTM D1525
Optical Properties
Original Value
Comments
Haze
50 %
@Thickness 1.00 mm
ASTM D1003
Gloss
85 %
@Thickness 1.00 mm
ASTM D2457
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
SCG Chemicals EL-Pro™ P700J Polypropylene Injection Molding
SCG Chemicals EL-Pro™ P600F Polypropylene Film Resin
PSCGC969 / 120723
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.