MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

LyondellBasell Montell 16501F7 Butene LLDPE  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblock

Applications: can liners and trash bags, blends, thin films

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: 16501 butene LLDPE film resin combine ease of processing with excellent optics and high film strength. These resins are well suited to replace LLDPE/LDPE blends in blown film applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirmnets of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.916 g/cc0.0331 lb/in³ASTM D792
Thickness 25.4 microns1.00 mil
Melt Flow 0.95 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.95 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiASTM D882
Film Elongation at Break, MD 800 %800 %ASTM D882
Film Elongation at Break, TD 1000 %1000 %ASTM D882
Secant Modulus, MD 0.179 GPa26.0 ksiASTM D882
Secant Modulus, TD 0.193 GPa28.0 ksiASTM D882
Elmendorf Tear Strength MD 150 g150 gASTM D1922A
Elmendorf Tear Strength TD 450 g450 gASTM D1922A
Elmendorf Tear Strength, MD 5.91 g/micron150 g/milASTM D1922A
Elmendorf Tear Strength, TD 17.7 g/micron450 g/milASTM D1922A
Dart Drop 4.13 g/micron105 g/milASTM D1709
Dart Drop Test 105 g0.232 lbASTM D1709A
Film Tensile Strength at Break, MD 42.1 MPa6110 psiASTM D882
Film Tensile Strength at Break, TD 30.3 MPa4390 psiASTM D882
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMO546 / 53671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.