MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Pearlstick™ 5715 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlstick™ 5715 is an aromatic polyester-based thermoplastic polyurethane.

Main Application: Solution coating

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccISO 2781
Brookfield Viscosity 100 - 200 cP20% T.S. in THF, RVT Spindle #2, 20 RPM, 23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ISO 868
Hardness, Shore D 49ISO 868
Tensile Strength 54.0 MPaISO 527-2/5A/200
Elongation at Break 290 %ISO 527-2/5A/200
50% Modulus 9.00 MPa
@Strain 50 %
ISO 527-2/5A/200
100% Modulus 12.0 MPa
@Strain 100 %
ISO 527-2/5A/200
Tear Strength 75.0 kN/mUnnicked; ISO 34-1B
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 °CKofler

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR5013 / 238883

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.