MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® D2109 DS-W (SBS) Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form identified:
Kraton D2109 DS-W - supplied as a dense, white pellet

Region: North America, Europe, Asia Pacific, Japan, and South America

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; and Impact Modification

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.915 - 0.945 g/cc0.915 - 0.945 g/ccBAM 1014
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm0.025 - 0.027 in/in
Melt Flow 14 - 24 g/10 min
@Load 5.00 kg,
Temperature 200 °C
14 - 24 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 5040 - 50Value of product compression molded 120°C; BAM 1003
Tensile Strength 3.45 MPa500 psiMachine Direction, typical properties Injection molded plaques, Die C; ASTM D412
 4.83 MPa701 psiTransverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
Elongation at Break 550 %550 %Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
 800 %800 %Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
100% Modulus  1.03 MPa
@Strain 100 %
149 psi
@Strain 100 %
Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
 1.38 MPa
@Strain 100 %
200 psi
@Strain 100 %
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
300% Modulus  1.72 MPa
@Strain 300 %
249 psi
@Strain 300 %
Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
 2.07 MPa
@Strain 300 %
300 psi
@Strain 300 %
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
Tear Strength 21.9 kN/m125 pliTransverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
 26.3 kN/m150 pliMachine Direction, typical properties Injection molded plaques, Die C; ASTM D412
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 182 °C340 - 360 °F
Middle Barrel Temperature 177 - 193 °C350 - 380 °F
Front Barrel Temperature 188 - 199 °C370 - 390 °F
Mold Temperature 10.0 - 37.8 °C50.0 - 100 °F
Injection Pressure 3.549 - 4.928 MPa514.7 - 714.7 psi
Back Pressure 0.276 - 0.414 MPa40.0 - 60.0 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D2109 DS-N (SBS) Compound
Kraton® D2122 DO (SBS) Compound
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer
Kraton® D1160 E (SIS) Linear Triblock Copolymer

PKRA9841 / 132740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.