MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Matexcel NAT-0042 Water soluble Crab Shell Chitosan
Categories: Wood and Natural Products

Material Notes: water soluble; chitosan; wound care; ntibacterial products; body care

Application: 1. It is used to prepare wound and burn dressings, with excellent hemostasis effect. 2. It can be made into capsule health products for body care. 3. It can be used as an absorption enhancer for hydrophilic drugs and natural nutritional cosmetics. 4. It has good film-forming and antibacterial properties, and can be used as additives and preservatives for food, fruits and vegetables.

Morphology: White to off white powder

Key Words: Source: Crab Shell
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 80 Mesh80 Mesh
Viscosity <= 50 cP<= 50 cP
Storage Temperature 20.0 °C68.0 °F
 
Descriptive Properties
Product overviewThis product is produced from crab shell. Water-soluble chitosan is processed through a special process, which improves the solubility of ordinary chitosan and maintains the high molecular properties of chitosan, making it more convenient to use and more widely used.Deacetylation: >93%
SolubilityWater

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1041 / 299672

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.