MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 SUPER-STA M NLGI No.1
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C.V. joints, U-joints, and brake self-adjusting screws found in passenger cars, trucks, agricultural machinery and industrial equipment. They are also recommended for other applications that call for an EP lithium grease. Super-STA M Grease is composed of Super-STA Grease, with the addition of Molybdenum Disulfide (Moly). It meets Mack MG-C performance requirements for a chassis lubricant. Moly is used to reduce wear by maintaining lubrication under conditions of high friction and shock loads. Super-STA and Super-STA M Greases are manufactured with high viscosity-index paraffinic base oils thickened with lithium 12-hydroxy stearate soap stock. They contain rust and corrosion inhibitors, an effective EP additive and a tackiness agent. This additive combination results in quality greases which ensure excellent lubrication and longer bearing life.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 95Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 880 SUSBase Oil Property
Saybolt Viscosity at 210°F 86 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 190 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 17 cStBase Oil
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 50
Four Ball Extreme Pressure, Weld Load 315 kg
Four Ball Wear 0.420 mm
Penetration P(60), 1/10 mm 325
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 275 °F
Minimum Service Temperature, Air -5.00 °F
Pour Point 10.0 °F(Base Oil Property)
Dropping Point 375 °F
 
Descriptive Properties
ASTM Rust A&BPass
ColorGray/Black
Low Temperature Mobility0.1 gm/secat 0°F
 0.2 gm/secat 10°F
 0.4 gm/secat 20°F
Oil Separation2.4 wt. %
Roll Stability5% Change
Shear Stability0% Change
Soap Type (Thickener)Lithium
Wheel Bearing Leakage0.7% Loss

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON222 / 75259

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.