MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubriplate 68-P Semi-Synthetic Refrigeration Compressor Oil
Categories: Fluid; Lubricant

Material Notes: These highly refined lubricants are formulated for use in refrigeration compressor systems utilizing ammonia, CFC (chlorofluorocarbon) and HCFO (hydrochlorofluorocarbon) refrigerants such as R-717, R-11, R-12, R-13, R-113, R-114, R-115, R-22, R-123, R-141b, R-142b, R-500, R-501 and R-502. They are not recommended for use with HFC (hydrofluorocarbon) refrigerants such as HFC-134a (R-134a).

Refrigeration Compressor Oils 68N & 68P are available in Pails & Drums.

Information provided by Lubriplate

Key Words: Part Number L0843-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 68ISO Grade
 106Viscosity Index
Saybolt Viscosity at 100°F 315 SUS
Saybolt Viscosity at 210°F 42 SUS
Kinematic Viscosity at 40°C (104°F) 63 cSt
Kinematic Viscosity at 100°C (212°F) 9.0 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -38.0 °F
Flammability Test 510[°F] Fire Point
Flash Point 468 °F
 
Descriptive Properties
SAE No.20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gabriel Fluorolube® GR-290 CTFE Fluoropolymer Grease
ExxonMobil Exterex™ A34 Synthetic Fluid
Dow MOLYKOTE® 1292 LONG LIFE BEARING GREASE
Nye Lubricants UniFlor 8310 (472) (UF) Synthetic Oil
Gabriel Versamid® 280B75 Polyamide Resin

WLUBR029 / 76075

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.