Product Description: 33% Glass Fiber, Heat Stabilized, Polyamide 66 Resin ID (ISO 1043): PA66-GF33 Filler/Reinforcement: Glass Fiber, 33% Filler by Weight Additive: Heat Stabilizer Processing: Injection Molding Color: Natural Information provided by Petropol |