Characteristics: SYNTHOS PS GP 152 is general purpose polystyrene (GPPS) with excellent optical properties, gloss and increased heat resistance. It is a thermoplastic material designed for injection moulding, extrusion, thermoforming and blow extrusion. SYNTHOS PS GP 152 is a colorless plastic. Product has a form of cylindrical granules of diameter 2.5 to 6 mms. Product may contain small amounts of granulate finer than that mentioned above of irregular shapes. Presence of any mechanical impurities in the granulate is not allowed.Information provided by Synthos |